Belin Nau'in Clinch Edge
bayanin samfuran
An ƙera belunan jigilar kaya na Jiangsu Huada don buƙatun ƙarfe mai ƙarfi, waɗanda suka haɗa da juriyar zafi 1050°C, ƙarfin kaya 5kg/cm², da kuma rashin fashewa a saman yayin ɗaukar zafi mai yawa na dogon lokaci.
Muhimman fa'idodi:
Kauri diamita na waya mai kauri 3.0-5.0mm yana jure manyan sassan PM
Saman da ke da iskar oxygen (ƙarin taro
Garanti na hana fashewa (wanda ya dace da ISO 14644-1 Class 5)
Takaddun shaida:
√ ISO 9001:2015 | √ ASTM A480 | √ MPIF Standard 35
Amfanin Fasaha
√ Juriyar Zafi Mai Girma
Kayan aiki: 314/310S Bakin Karfe
Ci gaba da aiki: 800-1050°C (H₂/N₂ yanayi)
Zagayen zafi: Zagayen 2000+ (ASTM E606)
√ Ƙarfin Nauyi Mai Nauyi
Diamita na waya: 3.0-5.0mm (wanda za'a iya gyarawa)
Matsayin kaya: Har zuwa 5kg/cm² (idan aka kwatanta da 3kg/cm² ma'aunin masana'antu)
Ƙarfin tauri: 800-1000 N/mm²
√ Daidaiton Iskar Oxidation
Mannewa a saman Layer na oxide: Matsayi A (ASTM D3359)
Karin yawan taro:
Zubar da ƙwayoyin cuta marasa tsari (ISO 14644-1 Aji 5)
Yanayin Aikace-aikace
| Tsarin PM | Kalubale | Maganin Huada |
| Sintering Mai Yawan Lodi | Canzawa a ƙarƙashin sassa masu nauyi | Waya 5.0mm + ƙarfafa sandar giciye |
| Tsaftace Tsaftace Zafi Mai Tsayi | Gurɓatar iskar shaka a saman | 310S tare da Layer ɗin oxide mai ƙarfi |
| Canja wurin Manyan Sassan PM | Ragewar raga | Tsarin ƙira na waya mai girman 4.5mm @ 50mm |
| Tsabtace Sintering | Gurɓatar iskar oxide | An yi amfani da na'urar lantarki mai gogewa ta Ra ≤0.6μm |
Sigogi na Fasaha
| Sigogi | Belt na Huada PM | Ma'aunin Masana'antu |
| Matsakaicin Yanayin Aiki | 1050°C | 750°C |
| Ƙarfin Lodawa | 5kg/cm² | 3kg/cm² |
| Riba ta Mass na Oxidation | 3-5mg/cm² | |
| Zaɓuɓɓukan Diamita na Waya | 3.0-5.0mm | 2.0-4.0mm |
Nazarin Shari'a: Mai Kaya Kayan Aiki na PM na Motoci
Bayan ɗaukar bel ɗin Huada:
Sifili nakasassu tare da wayoyi 4.2mm ƙasa da nauyin 4.8kg/cm²
Babu gurɓataccen iskar oxygen a cikin giya 10,000 masu niƙa
An rage farashin gyara kashi 30% a cikin watanni 18